Skip to main content
Impactinator® Glass - IMPACTINATOR Spezifikation isang itim at puting background

IMPACTINATOR®

Pagtutukoy ng salamin

IMPACTINATOR Pagtutukoy ng Salamin

mga katangian

Densidad ng katawan2.46±0.03g/cm3
Koepisyente ng Pagpapalawak ng Thermal98.0±2X 10-7/°C
Paglambot Point829±10°C
Annealing Point605±10°C
Strain Point559±10°C
Ang Modulus ni Young75.7GPa
Gupitin ang Modulus30.6GPa
Ang Ratio ni Poisson0.24/
Vickers Hardness (pagkatapos ng CS)700MPa
Tigas ng Lapis>8H/
Dami ng resistivity9.2lg(Ω • cm)
Dielectric Constant8.1F/m
Refraction Index1.51
Fo-elastic Constant27.1nm / cm / MPa

MGA KATANGIAN NG OPTICAL

Refraction Index1.51
Fo-elastic Constant27.1nm / cm / MPa
Optical specification

Scratches

W ≦ 0.05mm = ok

W > 0.05mm = not ok

Bubbles

d ≦ 0.10mm = ok

d> 0.30mm = not ok

Banayad na transmisyon (550nm)=92.2%

Paglaban sa kemikal

ReagentKonsentrasyon(%)Orasna Temperatura (°C)Pagbaba ng timbang (mg / cm2)
NaOH5 %6 h95±0.50.75
HCl5 %24 h95±0.50.12
HF10 %20 min20±0.517.18

Dielectric constant (15-20oC)

Dalas (MHz)Dielectric constant (10-12 F / m)
0.0018.20
0.017.84
0.17.89
547.82
1637.71
2727.65
3817.60
4907.58
5997.55
9127.43
14997.34
19777.31
24667.29
29867.26